Evidence of damage in carbon fibre composite tiles joined to a metallic heat sink under high heat flux fatigue - CEA - Commissariat à l’énergie atomique et aux énergies alternatives Accéder directement au contenu
Article Dans Une Revue Journal of Nuclear Materials Année : 1998

Evidence of damage in carbon fibre composite tiles joined to a metallic heat sink under high heat flux fatigue

Résumé

The two years experience with Active Metal Casting flat bonds shows that this technology is suitable for the heat fluxes expected in Tore Supra (10 MW/m²). Tests were pursued up to 3330 cycles, with elements still functional. At higher heat fluxes, fatigue damage is observed, but the bond resists remarkably well with no tile detachment. Examination of such deliberately damaged bonds showed distributed cracking, proving the absence of any weak link. The limitations to those higher heat fluxes are more related to the design and the base materials than to the bond itself.
Fichier principal
Vignette du fichier
ARTICLE4_for_open.pdf (1.58 Mo) Télécharger le fichier
Origine : Fichiers produits par l'(les) auteur(s)

Dates et versions

cea-03134221 , version 1 (08-02-2021)

Identifiants

Citer

R Mitteau, P Chappuis, L Moncel, J Schlosser. Evidence of damage in carbon fibre composite tiles joined to a metallic heat sink under high heat flux fatigue. Journal of Nuclear Materials, 1998, 258-263, pp.972 - 977. ⟨10.1016/s0022-3115(98)00314-6⟩. ⟨cea-03134221⟩
54 Consultations
49 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More